L - Patch is functioning well with very little or no deterioration. |
|
M - Patch deterioration or moderate spalling, or both, can be seen around the edges. Patch material can be dislodged with considerable effort, causing some FOD potential. |
|
H - Patch has deteriorated to a state that causes considerable roughness or high FOD potential, or both. The extent of the deterioration warrants replacement of the patch. |